http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105074977-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-622 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate | 2014-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105074977-B |
titleOfInvention | Binder composition for secondary battery electrode and its manufacture method, slurry for secondary battery electrode compositionss, electrode for secondary battery and secondary cell |
abstract | It is an object of the invention to provide a kind of excellent binder composition for secondary battery electrode of ageing stability, which can provide the secondary cell that can suppress to be produced, had good High temperature storage characteristic and high-temperature cycle by the gas that residual monomer causes.The adhesive composition of the present invention includes at least one of particle shaped polymer, reductoness compound and its oxide, Yi Jishui, the particle shaped polymer is that the monomer mixture of (methyl) acrylate monomer comprising more than 145 DEG C of boiling point is polymerized, and the particle shaped polymer relative to 100 mass parts, the content ratio of (methyl) acrylate monomer that more than 145 DEG C of the boiling point is 1 × 10 ‑6 More than mass parts and 1500 × 10 ‑6 Below mass parts. |
priorityDate | 2013-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |