http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105051074-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1804 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 |
filingDate | 2014-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105051074-B |
titleOfInvention | The manufacture method of polymer |
abstract | It is an object of the invention to provide the method for the polymer of the monomer that a kind of residual quantity of surfactant in the polymer as target compound or discharge opeing is low and manufacture is with vinyl.The manufacture method of polymer of the present invention is characterised by, the operation monomer with vinyl being polymerized in water-medium in the presence of the salt and polymerization initiator that are included in the surfactant peptides as natural peptid-based surfactant;Relative to 100 mass parts of above-mentioned monomer, the ratio of above-mentioned surfactant peptides salt (I) is more than 0.0005 mass parts and is less than 0.1 mass parts. |
priorityDate | 2013-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |