titleOfInvention | Friction reducer and the method for reducing the haydite floating degree in pumping haydite concrete are floated in a kind of haydite suppression |
abstract | The present invention provides a kind of floating friction reducer of haydite suppression and the method for reducing the haydite floating degree in pumping haydite concrete.The method that the detection that the present invention provides characterizes the haydite floating index of haydite floating degree, using inverting the treatment measures vibrated, is inverted the secondary method beaten, simple and quick, credible result degree is high.The floating friction reducer of haydite suppression that the present invention provides; and it is applied to the method reducing the haydite floating degree in pumping haydite concrete; pumping resistance can effectively be reduced; improve pumping lubricant effect; improve pump rate; reduce pumping pressure, the slump of haydite concrete of the floating friction reducer of admixture haydite suppression is not less than 90% with the percentage ratio of the slump of haydite concrete not filling the floating friction reducer of haydite suppression. |