classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K23-52 |
filingDate | 2015-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105036140-B |
titleOfInvention | Method for reducing viscosity of silicon dioxide slurry |
abstract | The invention provides a method for reducing the viscosity of silicon dioxide slurry, which comprises the steps of adding sodium metaaluminate into the silicon dioxide slurry, and the weight ratio of the sodium metaaluminate and silicon dioxide is 0.1 to 2 in a thousand; performing mechanical stirring, and then adding 0.1 to 3 in a thousand by weight of dispersant based on the silicon dioxide, performing the mechanical stirring again. According to the method for reducing the viscosity of the silicon dioxide slurry, the viscosity of the silicon dioxide slurry can be reduced under the condition that the solid contain is not reduced and the dosage of a viscosity reducing agent is reduced, the obtained silicon dioxide slurry has good mobility; the method for reducing the viscosity of the silicon dioxide slurry is conducive to the delivering of a pump and drying, and avoids the waste of water resources and the waste of energy sources. |
priorityDate | 2015-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 34.