http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105004669-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N19-04 |
filingDate | 2015-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105004669-B |
titleOfInvention | A kind of method of direct measurement reinforcing rubber mechanical property |
abstract | The invention discloses a kind of method of direct measurement reinforcing rubber mechanical property, 1)Prepare the sample needed;2)The measurement of sample:2.1)Measurement is carried out on electron detachment testing machine, before measurement, first resets current force value, displacement, peak value on electron detachment testing machine, while being configured to test relevant parameter;2.2)With fixture by the 1st)Thin adhesive tape sample prepared by step is fixed on electron detachment testing machine, and is run;2.3)It is out of service after sample is broken, record yield strength, extensibility, tensile strength and the maximal force during this;2.4)Wadding glue sample is prepared into>6mm cylindric or rectangular-shape sample, in measuring its hardness number under Shao Er hardometers.This method can direct measurement combination glue mechanical property, be easy to make further further investigation to combining glue, and measuring method is simple to operate, easy, user of service's study is fast. |
priorityDate | 2015-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 17.