titleOfInvention | The preparation method of the micro passage reaction that nano titanium oxide is modified |
abstract | The invention provides a kind of preparation method of the micro passage reaction of nano titanium oxide modification:Standby after the micro passage reaction cleaning treatment of preparation transparent material;Titanium source is added in aqueous acid or ammonia, stirring forms nano titanic oxide sol;Nano titanic oxide sol is injected in the passage of standby micro passage reaction, stops 5~30min, then deionized water is injected cleaning in the passage of micro passage reaction, obtain the micro passage reaction of nano titanic oxide sol particle modification;After being placed on illumination under the infrared light supply of 500~1000W, use acid wash liquid, deionized water to be cleaned by ultrasonic passage successively, obtain final product the micro passage reaction of nano titanium oxide modification;Preparation method process is simple of the present invention, easily realizes industrialized production, and the micro passage reaction channel density of preparation is high, has convenient, efficient feature. |
priorityDate | 2015-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |