http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104934572-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1391 |
filingDate | 2015-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104934572-B |
titleOfInvention | A kind of preparation method of nickel cobalt aluminium lithium/titanium dioxide composite positive pole |
abstract | The present invention provides a kind of preparation method of nickel cobalt aluminium lithium/titanium dioxide composite positive pole, and this composite positive pole includes nickel cobalt aluminium lithium internal layer and TiO 2 Outer layer;Including step:Metal salt is configured to solution by metal ratio in internal layer nickel cobalt aluminium lithium material;Sprayed into after being atomized by atomizer in high temperature pyrolysis stove, obtain internal layer nickel cobalt aluminium lithium material;The internal layer nickel cobalt aluminium lithium material is added in the container equipped with titanium tetrachloride, is sufficiently stirred for, pulp, obtains mixed serum;Then dry, be calcined, broken, screening obtains nickel cobalt aluminium lithium/titanium dioxide composite positive pole.Nickel cobalt aluminium lithium/titanium dioxide composite positive pole product particle prepared by this method is single crystal grain, is evenly coated, component is homogeneous. |
priorityDate | 2015-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |