titleOfInvention | A kind of fishing poly butyric hydroxypentanoic acid copolyesters monofilament manufacture method |
abstract | A kind of fishing degradable poly hydroxybutyric acid hydroxypentanoic acid copolyesters monofilament manufacture method, the present invention adopts the fishing degradable poly hydroxybutyric acid hydroxypentanoic acid copolyesters monofilament that melt spinning, super drawing technique are obtained;Described poly butyric hydroxypentanoic acid copolyesters number-average molecular weight is 180000~200000;Described poly butyric hydroxypentanoic acid copolyester section baking temperature is 70~120 DEG C, and the time is 24~48 hours, and vacuum is 0.05~0.1MPa;Described melt spinning and super drawing technique are:Spinning temperature is 175~185 DEG C, and spinning speed is 5~50m/min, and draw ratio is 3~5 times, and drawing medium is hot bath, and draft temperature is 60~100 DEG C. |