http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104870694-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C59-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2059-023 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C59-022 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C59-02 |
filingDate | 2013-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104870694-B |
titleOfInvention | There is the manufacture method of the formed body of minute concave-convex structure and surface to have the formed body of minute concave-convex structure for the manufacture method of porous anodic aluminium oxide and surface |
abstract | The present invention relates to a kind of manufacture method of porous anodic aluminium oxide, it is characterised in that it is the manufacture method that the surface of aluminium base is formed with the porous anodic aluminium oxide of the oxidation overlay film with multiple pores, and this method includes:Process (a), aluminium base is immersed in and is mixed with a variety of sour electrolyte;Process (b), voltage is applied to the foregoing aluminium base being immersed in aforementioned electrolyte;Process (c), does not substantially apply voltage to foregoing aluminium base, keeps the state in the electrolytic solution by foregoing aluminium base dipping;And process (d), it is alternately repeated foregoing sequence (b) and foregoing sequence (c).The method that the surface that can be provided device easy to use according to the present invention and easily manufacture aluminium base with less process number is formed with the porous anodic aluminium oxide of the oxidation overlay film with multiple pores. |