Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-38 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-7007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-7038 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-7015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-36 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-02 |
filingDate |
2013-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c90ec98cf32419cdf73e2022b307e3f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a80d48e4902493e9d34944bad86090d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f9c5dc46c038f8df4d5faa14eb63009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31efafd8cf6d91ec2c448c0b5940cf62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b2170680eeb4a7a99e0eef5137a9c2da |
publicationDate |
2015-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-104854031-A |
titleOfInvention |
Post-treatment of zeolitic material |
abstract |
A process for the post-treatment of a zeolitic material comprises (i) providing a zeolitic material, wherein the framework structure of the zeolitic material comprises YO2 and X2O3, wherein Y is a tetravalent element and X is a trivalent element; (ii) subjecting the zeolitic material provided in (i) to a method comprising (a) treating the zeolitic material with an aqueous solution having a pH of at most 5, (b) treating the zeolitic material obtained from (a) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75 DEG C; wherein in (ii) and after (b), the zeolitic material is optionally subjected to at least one further treatment according to (a) and/or at least one further treatment according to (b). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111252781-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108946755-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111252781-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108778997-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108778997-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112188927-A |
priorityDate |
2012-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |