classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 |
filingDate | 2015-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104804128-B |
titleOfInvention | A kind of preparation method of nano-negative ion polyacrylate compound particle |
abstract | The present invention provides a kind of preparation method of nano-negative ion polyacrylate compound particle, and its preparation process is:The negative ion powder for weighing 100 parts is added in 100 200 parts of 95% ethanol, ultrasonic wave disperses after 30 60min, add 15 parts of silane couplers, 80 90 DEG C of stirring reactions 35 hours, modified Nano negative ion powder is dried in vacuo to obtain after suction filtration, nano-negative ion polyacrylate compound particle with core shell structure has been synthesized by pre-emulsification, in-situ emulsion polymerization, nano-negative ion polyacrylate compound particle prepared by the present invention is compared with the nanometer anion powder not being wrapped by, and the compound particle has excellent dispersiveness. |