titleOfInvention | A kind of nail polish and preparation method thereof |
abstract | The invention discloses a kind of nail polish and preparation method thereof, belong to cosmetic technical field.Described nail polish is by weight to add 15 30 parts of crushing natural film forming matters in 65 80 parts of volatile solvents, is uniformly dispersed with 100 300rpm rate of dispersion, obtains mixed material;Mixed material is stood to 36 56 hours at room temperature again, 0.5 8 parts of NMFs are finally added in mixed material, 3 5min are disperseed with 400 600rpm rate of dispersion;Described natural film forming matter reaches at least one of glue, rosin, shellac, gum dammar for agate base of a fruit natural gum, mountain.The nail polish of the present invention is water sample quality, and long-term use will not be to the toxic effect of human body, and surface drying time is within 1 minute at room temperature, film formation surface is smooth, gloss has more excellent adhesive force to first face more than 80 °, and the effect of maintenance nail is can reach while rapid nail art. |