http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104789038-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-101 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M1-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-101 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M1-12 |
filingDate | 2015-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104789038-B |
titleOfInvention | A kind of silk-screen printing technique |
abstract | A kind of silk-screen printing technique, comprises the steps successively:(1)Make screen printing forme;(2)Screen printing forme is installed, UV curable ink is added and is printed;UV curable ink used is by urethane acrylate, epoxy acrylate, tri (propylene glycol) diacrylate, three acrylic acid propane front three alcohol esters, 1, the phenylene of 1'(methylene 2 4,1) double [acetone of 2 hydroxyl, 2 methyl 1], polymerization [2 hydroxyl 2 methyl 1 [4 (1 methyl ethylene) phenyl] acetone], dimethyl silicone polymer, Siloxane-Oxyalkylene Copolymers and Tissuemat E composition;(3)Using the ultraviolet light that wavelength is 200-300 nanometers, make the top layer solidification of ink for screen printing layer;(4)Using the ultraviolet light that wavelength is 360-400 nanometers, make ink for screen printing layer solidification.The ink printed layer that the present invention is formed has wrinkle effect, good anti-yellowing property and good folding resistance. |
priorityDate | 2015-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |