http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104759599-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D11-22 |
filingDate | 2015-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104759599-B |
titleOfInvention | A kind of method utilizing shell thickness control system to improve strand temperature |
abstract | The invention provides a kind of method utilizing shell thickness control system to improve strand temperature, it is achieved water saving and UTILIZATION OF VESIDUAL HEAT IN, energy-saving and cost-reducing.The step of the method includes: by actual value, casting blank cross-section size, material, crystallizer parameter and covering slag parameter are inputted industrial computer; pressed solidification shell thickness model conventional value presetting each point intensity of cooling value by industrial computer, PLC send water distribution and instruct to each valve of cooling water system;By industrial computer dynamic acquisition observed temperature, PLC send water distribution and instruct to each valve of cooling water system;By industrial computer dynamic acquisition Actual Casting Speed, PLC send water distribution and instruct to each valve;By industrial computer dynamic acquisition and the follow-up intensity of cooling of control, until two side green shell contacts, i.e. arrive Coagulated hemothorax.The present invention can make continuous casting billet surface temperature at cut-out point improve 100 200 DEG C, and a set of casting machine producing million tons per year can save waste heat 1.0X10 every year 14 J, equivalent standard coal about 3000t. |
priorityDate | 2015-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 17.