http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104693546-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 |
filingDate | 2015-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104693546-B |
titleOfInvention | A kind of preparation method of High-performance graphite oxide alkene/solution polymerized butadiene styrene rubber composite |
abstract | The present invention relates to the preparation method of a kind of High-performance graphite oxide alkene/solution polymerized butadiene styrene rubber composite, belong to rubber composite field.The technique that the present invention utilizes solution polymerized butadiene styrene rubber emulsion to prepare, graphene oxide and solution polymerized butadiene styrene rubber emulsion compound, complex emulsions co-coagulation and mechanical blending combine prepares graphene oxide/solution polymerized butadiene styrene rubber composite, emulsion preparation technology is simple for solution polymerized butadiene styrene rubber, with low cost, emulsion is combined and makes graphene oxide is height stripping, high dispersion state.Graphene oxide/solution polymerized butylbenzene rubber master batch can with direct mechanical processing can also and with solution polymerized butadiene styrene rubber solid-state glue, also can mix other fillers and prepare high-performance solution polymerized butadiene styrene rubber nano-composite material.Solution polymerized butadiene styrene rubber composite prepared by this method can give play to the effect of graphene oxide to greatest extent, improves the mechanical strength of solution polymerized butadiene styrene rubber composite, wearability, anti-slippery, reduces heat etc..The present invention is simple, has a extensive future. |
priorityDate | 2015-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links