http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104673063-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-6958 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-695 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2015-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104673063-B |
titleOfInvention | High-temperature-resistant, anti-corrosion and thermal-insulation coating and preparation technology thereof |
abstract | The invention discloses a high-temperature-resistant, anti-corrosion and thermal-insulation coating which comprises components in parts by weight as follows: 45-60 parts of film-forming resin, 20-30 parts of a pigment and filler, 15-30 parts of an aid and 25-30 parts of a solvent. The invention further designs a preparation technology of the high-temperature-resistant, anti-corrosion and thermal-insulation coating. The technology comprises steps as follows: firstly, mixing the film-forming resin with the pigment and the filler, sequentially adding an antifoaming agent, a leveling agent, a coupling agent, a crosslinking agent and a curing agent, and evenly stirring the mixture at the normal temperature to obtain the high-temperature-resistant, anti-corrosion and thermal-insulation coating. The coating has the advantages of environment-friendliness, low cost, high hardness, long service life, good heat resistance, good flexibility, good high-temperature resistance and the like. |