http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104624383-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D101-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B03D1-016 |
filingDate | 2014-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104624383-B |
titleOfInvention | Hematite reverse flotation inhibitor and preparation and use method thereof |
abstract | The invention relates to a hematite reverse flotation inhibitor and a preparation and use method of the hematite reverse flotation inhibitor. The hematite reverse flotation inhibitor is prepared by waste residues generated in the beer brewing process, potassium permanganate, sodium hydroxide and water, and according to the weight ratio of all the components, the waste residues: potassium permanganate: sodium hydroxide: water is 1: five percent to 20 percent: four percent to 20 percent: 80 percent to 120 percent. The hematite reverse flotation inhibitor is easy to prepare, good in floating effect and small in use number, the defect of sodium hydroxide as the inhibitor is overcome, normal temperature preparation is achieved, the selectivity of the inhibitor is improved, then the iron recycling rate is improved, the use number of inhibitors is reduced, the needs of dressing production are met, the guaranteeing degree of iron ore resources in China to the iron and steel industry is improved, and immoderate reliance on grain and consumption of the grain are reduced. |