http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104593116-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E50-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10L5-48 |
filingDate | 2015-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104593116-B |
titleOfInvention | Biomass liquefying residue prepares the method for solid molding fuel |
abstract | The invention discloses a kind of method that biomass liquefying residue prepares solid molding fuel, the method includes mixing biomass liquefying residue, binding agent and auxiliary fuel, the moisture content of gained mixing raw material is regulated to 10%~20%, the most extruded, obtain solid molding fuel.The method of the present invention can realize the recycling of liquefied residue, the solid molding fuel density that obtains is high, intensity is big, calorific value is high, anti-water absorbing capacity is strong, with low cost, energy-conserving and environment-protective, achieve the solid waste recycling with biomass, can effectively solve the process handling problems of solid waste and biomass. |
priorityDate | 2015-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 63.