classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2400-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J13-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K5-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J13-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F230-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K5-06 |
filingDate | 2014-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104592803-B |
titleOfInvention | Organic-silicon-modified phase-change microcapsule and preparation method thereof |
abstract | The present invention relates to a kind of organic-silicon-modified phase-change microcapsule and preparation method thereof, building coating is can be applied to, it is prepared by the raw material that following weight matches according to following the step of sequentially carrying out:1) pre-emulsification:50 70 parts of paraffin, 14 19 parts of styrene, 0.3 1 parts of organosilicon modifiers, 5 8.5 parts of methacrylic acids, 55 82 parts of deionized waters, 24 parts of anion emulsifiers, 0.5 1.5 parts of nonionic emulsifiers and 0.25 1 parts of initiators are added in pre-emulsification reactor, at a temperature of higher than 3 15 DEG C of melting point of paraffin wax, under 800 1200r/min rotating speeds disperse, pre-emulsification 10 40 minutes, obtains pre-emulsion;2) emulsion polymerization;3) post-process;It can improve the stability of phase-change microcapsule polymer emulsion, reduce the collision cohesion between phase-change microcapsule emulsion particle, improve dispersiveness of the emulsion particle in coating. |
priorityDate | 2014-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |