http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104559914-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J171-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-06 |
filingDate | 2015-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104559914-B |
titleOfInvention | A kind of Sealant room temperature vulcanization dealcoholysis silicone rubber and preparation method thereof |
abstract | The invention discloses a kind of Sealant room temperature vulcanization dealcoholysis silicone rubber and preparation method thereof, the silicone rubber of the present invention consists of by weight: α, alpha, omega-dihydroxy polydimethyl siloxane 40-80 part;MS polymer 1-50 part;Calcium carbonate 5-120 part;Cross-linking agent 2-20 part;White carbon 1-20 part;Coupling agent 0.1-5 part;Catalyst 0.01-1 part;The present invention improves Sealant by MS polymer, and by α, alpha, omega-dihydroxy polydimethyl siloxane, MS polymer and calcium carbonate stir in kneader;Add cross-linking agent to be sufficiently stirred for;Add white carbon to be sufficiently stirred for;After addition coupling agent and catalyst are sufficiently stirred for, plastic emitting obtains product.The present invention improves the Sealant performance of silicone rubber. |
priorityDate | 2015-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links