classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-10 |
filingDate | 2015-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104530510-B |
titleOfInvention | The preparation technology of the poly-butyronitrile special-purpose nanometer short fiber material of breast |
abstract | The present invention relates to the preparation technology of a kind of breast poly-butyronitrile special-purpose nanometer short fiber material, comprise the steps: step (1), by attapulgite coarse crushing, spray silane coupler, water spray, be squeezed into lamellar attapulgite;Step (2), stacks described lamellar attapulgite, described lamellar attapulgite and water is put into rustless steel troughing, adds dispersant composition, making beating, high speed shear, then high pressure homogenize processes, it is thus achieved that emulsion;Step (3), is dehydrated described emulsion by after cyclone classification, it is thus achieved that biscuit;Step (4), dries described biscuit, broken, adds stearic acid, pulverizing, comminution by gas stream, obtains newborn poly-butyronitrile special-purpose nanometer short fiber material.The operating procedure of the present invention is simple, is easily controlled, low cost, is suitable to industrially large-scale application. |
priorityDate | 2015-01-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |