http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104513347-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F293-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 |
filingDate | 2014-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104513347-B |
titleOfInvention | The method that soft nanometer coupling technology prepares composite nanometer particle |
abstract | The method that soft nanometer coupling technology prepares composite nanometer particle, to AIBN, CPADB and solvent is added in the first monomer, is passed through Ar or N 2 , purification obtains Macro RAFT agent after carrying out RAFT reactions;Second monomer, AIBN and solvent are added, Ar or N is passed through 2 , purification obtains bi-block copolymer after being reacted;The third monomer, AIBN and solvent are added, Ar or N is passed through 2 , purification obtains triblock polymer after being reacted;α LA, TBAB and THF are added, Ar or N is passed through 2 , react the triblock polymer for obtaining alpha lipoic acid modification;It is added dropwise to after reacting in the THF solution of Au NPs and adds SiO 2 The THF solution of NPs, reaction is obtained.Present invention, avoiding the complicated inorganic embedding step of multistep and the experiment condition of harshness, cost is reduced. |
priorityDate | 2014-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links