abstract |
The present invention provides a kind of polyacetal resin composite, it comprises polyacetal resin (A) and polyvinyl resin (B), the polyacetal resin (A) mixing ratio shared by the gross mass of polyacetal resin (A) and polyvinyl resin (B) is 10~90 mass %, polyacetal resin (A) with 190 DEG C, the melt flow rate (MFR) that the condition of 2.16kg load measures is less than 30g/10 minute, polyvinyl resin (B) is made up of modified polyvinyl resin, in the case of the gross mass of polyvinyl resin is designated as 100 mass %, degree of modification is more than 0.01 mass %, polyvinyl resin (B) with 190 DEG C, the melt flow rate (MFR) that the condition of 2.16kg load measures is less than 2.5g/10 minute. |