classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 |
filingDate | 2014-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104439231-B |
titleOfInvention | A kind of Au modifies the preparation method of Zn/ZnO micro Nano material |
abstract | The invention belongs to micro-nano technical field of function materials, particularly a kind of electrochemical deposition is combined with displacement method and prepares the method that Au modifies Zn/ZnO micro nano structure functional material.On substrate silicon chip, parallel placement two electrodes, drip ZnSO in-between the electrodesn 4 electrolyte, cover sheet glass, be positioned over moist closet, the TEC of moist closet is utilized to make to form an ice sheet be covered with between two electrodes between silicon chip and sheet glass, place 30 minutes again at moist closet, the DC voltage then adding 0.8 ~ 1.4V between electrodes deposits 30 minutes, and products therefrom washed with de-ionized water to be dipped in chlorauric acid solution 30 seconds after drying, take out again, clean, dry, just obtain Au and modify Zn/ZnO micro nano structure.The present invention is simple to operate, and the product of preparation has higher surface reinforced Raman active, and can reuse. |