abstract |
Problem of the present invention is to provide the few and regenerated fiber from amenities of aesthetic appearance, strength characteristics excellence of a kind of field trash.Carry out regenerating process to the amenities containing cellulose pulp and outward appearance that the amount of Ultrahigh water absorbent polymer (SAP) that obtains is less than the regenerated fiber self of the regenerated fiber of 10% is good, use the aesthetic appearance of the products formed of regenerated fiber, strength characteristics also excellent.And, as regenerated fiber, preferably to use the inclusion area rate of cobalt chloride (II) hexahydrated Determination Staining for 50000mmn 2 / mn 2 below, and Canadian Standard Freeness is more than 600ml. |