http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104396055-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-139 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-583 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-04 |
filingDate | 2013-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104396055-B |
titleOfInvention | Method for the positive electrode active materials for producing carbon coating |
abstract | This application discloses a kind of methods for producing positive electrode active materials.In order to produce positive electrode active materials, raw material is mixed in polyol solvent with reaction of formation solution, is then burnt to generate the first positive electrode active material powder.Then, first positive electrode active material powder is coated using flammable organic solvent, is then burnt to generate the second positive electrode active material powder.The positive electrode active materials produced with this method have improved capacity and crystallinity. |