http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104387865-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2206 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-12 |
filingDate | 2014-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104387865-B |
titleOfInvention | A kind of high temperature modification fluorubber elastic wear-resisting coating and preparation method thereof |
abstract | The present invention relates to coating material technical field, mainly for the preparation of metal-rubber composite board material, being specially a kind of high temperature modification fluorubber elastic wear-resisting coating and preparation method thereof, this high temperature modification fluorubber elastic wear-resisting coating includes 100 parts of crude fluororubber, 5 parts of acid-acceptors, 5 lubrication fillers, 2 parts of vulcanizing agents, 10~30 parts of cross-linking agent, 2~5 parts of organic amine curing agent and 500~800 parts of organic solvents.This high temperature modification fluorubber elastic wear-resisting coating through banburying, irradiation, dissolve and filtration is made.The fluororubber coating wear-resisting intensity of gentleness corrosion-resistant, resistance to using the present invention to prepare is high, cold curing speed, and its preparation method production technology is simple, with low cost. |
priorityDate | 2014-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.