http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104368367-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W10-37 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-18 |
filingDate | 2014-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104368367-B |
titleOfInvention | A kind of Graphene/hydroxyl cupric phosphate composite catalyst and preparation method thereof |
abstract | The invention belongs to the preparation field of composite catalyzing material, be specifically related to a kind of Graphene/hydroxyl cupric phosphate composite catalyst and preparation method thereof.Concretely comprise the following steps: 1) prepare the graphene oxide water solution of certain solubility;2) a certain amount of graphene oxide water solution is added in soluble copper salt and soluble phosphate reaction system;3) regulation pH value;4) above-mentioned suspension is placed 100 ~ 140 DEG C of reaction 6 12h in a kettle., cool down, be centrifuged, wash after dry to obtain Graphene/hydroxyl cupric phosphate composite catalyst.In composite catalyst, the mass ratio of graphene nanometer sheet and hydroxyl cupric phosphate is 0.2~6% 99.8~94%, and ratio of greater inequality is 2% 98%.This composite catalyst has good catalytic performance under simulated solar irradiation, can be applicable to the water treatment field of industrial wastewater. |