http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104356581-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A43B13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 |
filingDate | 2014-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104356581-B |
titleOfInvention | A kind of anti-wet skid thermoplastic shoe sole and preparation method thereof |
abstract | The present invention relates to the technical field of polymer materials, and provides a kind of anti-wet skid thermoplastic shoe sole with high wet skid resistance, good low temperature flexibility and dimensional stability, which can be recycled repeatedly and improves environmental protection effect, and a preparation method thereof. The anti-slip thermoplastic shoe sole consists of the following components: styrene-butadiene-styrene block copolymer (SBS), epoxidized styrene-butadiene-styrene block copolymer (ESBS), acrylonitrile- Styrene-acrylate copolymer (ASA), white mineral oil, antioxidant, ultraviolet absorber, zinc stearate, nano-calcium carbonate, premix the above component materials in a high-speed mixer for 4-7 minutes, then The premixed material is passed through a twin-screw extruder, melted and extruded at 130-135 degrees, cooled and granulated, and finally injected at 168-172 degrees to obtain the anti-wet skid thermoplastic shoe sole. |
priorityDate | 2014-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |