http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104350010-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C05D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C05B17-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01D13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C05D9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C05D9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C05D1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B39-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C05G1-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C05G1-00 |
filingDate | 2014-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104350010-B |
titleOfInvention | Alkali metal ion sources and methods of formation with moderate ion release rates |
abstract | A source of alkali metal ions having a moderate release rate of ions (such as potassium) formed by a process comprising the steps of: 1) adding a granular ore (such as orthosilicate) containing at least one frame silicate bearing alkali metal ions rock ore) combined with at least one of oxides and hydroxides of at least one of alkali metals and alkaline earth metals, such as calcium hydroxide; 2) grinding a mixture of these two components optionally with water, optionally grinding separately and drying and then optionally blended with water; 3) if no water was added prior to grinding, a mixture is formed by adding water to the solid mixture after grinding; 4) exposing the mixture to elevated temperature and pressure to form a gel comprising the framework silicate of silica and alkali metal. |
priorityDate | 2013-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |