http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104327225-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F292-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-588 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-524 |
filingDate | 2014-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104327225-B |
titleOfInvention | Nano SiO2 composite material thickened oil viscosity reducer and preparation method thereof |
abstract | The invention discloses a nano SiO2 composite material thickened oil viscosity reducer and a preparation method thereof, which belongs to the technical field of nano SiO2 composite material preparation and application thereof. The viscosity reducer is nano (polymethacrylate higher alcohol-acrylamide)/SiO2 composite material. The preparation method comprises the following steps: 1)pre-modifying the surface of the nano SiO2 by a silane coupling agent; and 2)performing graft copolymerization of (methyl)acrylate higher alcohol and acrylamide on the surface of nano SiO2 to obtain the (polymethacrylate higher alcohol-acrylamide)/SiO2 composite material powder. The nano viscosity reducer has the advantages of good viscosity reducing effect, low cost, simple production and no pollution during a cleaning process. Through the experiment, the viscosity reducing rate of the nano viscosity reducer to the high wax thickened oil at Daqing dandong station is 72.10% at 40 DEG C. |
priorityDate | 2014-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links