Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2203-318 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2483-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-1457 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-0075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-401 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-385 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-00 |
filingDate |
2013-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2017-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2017-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-104321397-B |
titleOfInvention |
Adhesive article |
abstract |
The present invention includes adhesive article, adhesive composition and release liner.The release liner includes the barrier formulation based on siloxanes, the barrier formulation can provide for changing and processing the Average peel force and electrostatic peeling force needed for flexible adhesives, specifically for the Average peel force and electrostatic peeling force needed for the binding agent of the type in electronics industry.In one embodiment, the preparation based on siloxanes includes the addition curing barrier formulation based on siloxanes. |