http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104312158-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_22d2ae43bd5a5dc7f9e132b8a6084ce0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-18 |
filingDate | 2014-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd963592b323c01e75f669bbe12990fb |
publicationDate | 2015-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104312158-A |
titleOfInvention | Preparation of silicone rubber for dealcoholization at room temperature |
abstract | The invention discloses preparation of silicone rubber for dealcoholization at room temperature. The preparation method comprises the following steps of: carrying out vacuum drying for 4 hours on spherical aluminum oxide powder in a vacuum drying box with the temperature of 120 DEG C, and cooling to room temperature for spare use; adding 80 parts of methyl dimethoxy silane-terminated polydimethylsiloxane, 5-8 parts of spherical aluminum oxide, 5-8 parts of methyltrimethoxysilane, 1-3 parts of D-60, 1-3 parts of KH-550, 0.1-1 parts of dibutyltin dilaurate in parts by weight in sequence into a planetary kettle; and carrying out vacuum mixing for 1-2 hours. |
priorityDate | 2014-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.