titleOfInvention | Environment-friendly water-based crackle paint and using method thereof |
abstract | The invention provides a kind of environment-friendly water-based crackle paint and using method thereof, including aqueous crackle priming paint and aqueous crackle finish paint, described aqueous crackle priming paint includes following components count by weight percentage: waterborne epoxy modified acrylic resin 20~30%;Nertralizer 0.5~1.5%;Firming agent 10~20%;Cosolvent 10~20%;Levelling agent 0.01~0.1%;Defoamer 0.01~0.1%;Catalyst 0.01~0.1%;Aqueous color paste 10~20%;Water 10~30%, described aqueous crack surface enamel-cover includes following components count by weight percentage: styrene-acrylic emulsion 60~80%;Nertralizer 1~2%;Aqueous color paste 15~40%;Aqueous crackle agent 0.01~0.1%.Compared with correlation technique, the present invention has the beneficial effects that, environmental protection, security performance are higher, and decorative effect is preferable, and adhesive force is stronger. |