http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104167949-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H02N1-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H02N1-04 |
filingDate | 2013-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104167949-B |
titleOfInvention | The manufacture method of friction generator and friction generator |
abstract | The manufacture method of friction generator and friction generator.The method comprises: 1) prepare burden: the slurry preparing macromolecular material; 2) be coated with: described slurry is coated in flat panel substrates equably; 3) dry solidification: carry out dry solidification process to the base material being coated with slurry, obtains macromolecule membrane layer-substrate layer duplexer; 4) hot padding is added: to 3) dry solidification step gained macromolecule membrane layer-substrate layer duplexer heats and embossing process, obtains the macromolecule membrane layer-substrate layer duplexer with micro-nano concaveconvex structure; And 5) assembling: according to 4) macromolecule membrane layer-substrate layer duplexer of obtaining of heating imprint step makes friction generator.The manufacture method of friction generator provided by the invention can produce friction generator easily, and manufacture process is simple, and cost is low. |