http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104119028-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-42 |
filingDate | 2014-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104119028-B |
titleOfInvention | The multi-functional toughener of anti-crack and anti-seepage |
abstract | The invention discloses the multi-functional toughener of a kind of anti-crack and anti-seepage, it is mixed by the raw material of following weight part: Orlon 10-15, hydroxyapatite powder 18-24, perfluoro octane sulfonate 5-10, JF-6 type early strength water-reducing agent? 25-35, sodium polyacrylate 12-18, furan mastic powder 5-10, CH3-(CH2)13N(CH3)2-O 3-6, SC-11 type polycarboxylate water-reducer? 18-26, refining slag 10-15, trisodium phosphate 4-8, pentaerythritol stearic acid ester 2 3-5, N-oleoyl-N methyl taurine sodium 5-8, aluminium borate whisker 6-12, polyoxyethylene glycol 5-10, amido silicon oil 7-11, zinc palmitate 2.5-4.5, auxiliary agent? 4-6.The multi-functional toughener of anti-crack and anti-seepage of the present invention is compared with common toughener, reaction more rapidly, more complete, gain in strength sooner, higher, concrete wear-resisting, durable cracking resistance and barrier performance can be significantly improved, and also there is the effect of diminishing, early strong, bleed, stronger for various concrete adaptability, have a extensive future. |