http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104098767-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-10 |
filingDate | 2014-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104098767-B |
titleOfInvention | The preparation method of polyaniline and ring oxygen grafted and mofiied acrylic ester mixture |
abstract | The preparation method of polyaniline and ring oxygen grafted and mofiied acrylic ester mixture, relate to coating material production technical field, in the presence of a solvent, first epoxy resin, function monomer, acrylate and initiator mixing are prepared carboxylic epoxy grafted acrylate ester resin by solution polymerization process; Then add aniline, carboxylic epoxy grafted acrylate ester resin carries out the in-situ oxidizing-polymerizing of aniline, obtain polyaniline-ring oxygen grafted and mofiied acrylic ester mixture. The ring oxygen grafted and mofiied acrylic ester resin formed concentrated the room-temperature-curable performance of epoxy resin, antiseptic property excellent and with the feature such as the strong adhesion of base material, and acrylate resin is water-fast, weather-proof, protect the features such as light, Bao Se and mechanical property adjustability. Mixture in organic solvent with molecular level state compound, long-term shelf-stable. |
priorityDate | 2014-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 54.