titleOfInvention | High-temperature-resistant wear-resistant anti-corrosive composite material sucker rod and preparing method |
abstract | The invention discloses a high-temperature-resistant wear-resistant anti-corrosive composite material sucker rod. A high-temperature-resistant wear-resistant anti-corrosive layer is arranged on the outer circumferential surface of the oil sucker rod and is made of polyimide materials; and the sucker rod and polyimide are bonded through coupling agents and bonding agents. The high-temperature-resistant wear-resistant anti-corrosive composite material sucker rod has the advantages that the bonding intensity is high; peeling cannot easily occur; scale formation and wax accumulation are avoided; the sucker rod can withstand the high temperature of 200 DEG C to 300 DEG C; the long-time use can be guaranteed; the pipe rod eccentric wearing possibility under the high-temperature condition can be greatly reduced; and the service life of the sucker rod is prolonged. |