http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104071997-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-24 |
filingDate | 2014-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104071997-B |
titleOfInvention | Comprehensive utilization red mud, ardealite and the method for gangue |
abstract | Comprehensive utilization red mud, ardealite and the method for gangue, it is to be main raw materials and fuel with red mud, ardealite, gangue, being aided with correction material is secondary raw materials and fuel, homogenizing is produced containing wet stock with two-stage batching technique, homogenizing through molding or is dried broken containing wet stock, then, produced containing dicalcium silicate, calcium sulphoaluminate and grog product that sulfur calcium ferrite is main component by calcining.The grog that the inventive method prepares, directly can sell as product;Prior art can also be utilized, be processed into Binder Materials further or goods are sold.The inventive method technique is simple, it is little to invest, production scale is the most changeable, the high-early-strength grog purposes produced according to the inventive method is wide, and it is worth higher, not only save substantial amounts of clay resource and non-renewable fire coal, and can effectively dissolve waste pollutant and to the pollution of environment and prevent secondary disaster, there is industrial competitiveness and good investment economy. |
priorityDate | 2014-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 38.