http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104024309-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2309-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2307-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-203 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-548 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 |
filingDate | 2012-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104024309-B |
titleOfInvention | Manufacture method, the rubber composition of rubber composition and use its pneumatic tire |
abstract | A kind of manufacture method of rubber composition is provided, described rubber composition is by by rubber components (A), the filler that contains inorganic filler (B), silane coupler (C) and at least one vulcanization accelerator (D) compounding that is selected from specific compound form, described rubber components (A) comprises natural rubber and/or synthetic diene series rubber, described method is characterised in that described rubber composition carries out mixing in multiple stages: in the mixing first stage (X), add a part (A ˊ) of described rubber components (A), all or part of described inorganic filler (B), all or part of described silane coupler (C) and all or part of described vulcanization accelerator (D), and together mixing, with in mixing subsequent stage, add the remainder (A ") together mixing of described rubber components (A). thereby this manufacture method can increase the coupling function of silane coupler, active acquisition advantageously has low febrifacient rubber composition. |