classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-58 |
filingDate | 2014-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-104004430-B |
titleOfInvention | A kind of fast light preparation method with germ resistance water soluble acrylic acid esters resin coating |
abstract | The present invention relates to a kind of fast light preparation method with germ resistance water soluble acrylic acid esters resin coating, it is characterized in that: add water, emulsifying agent, vinylformic acid, be warming up to 45 DEG C, stir 45min, add A monomer, anti-bacterial material and cationic polyacrylamide, emulsification 40 ~ 60min, be warmed up to 80 DEG C of insulations, drip initiator B, time for adding 0.5 ~ 2.5h, drip reaction 2h, obtain stratum nucleare emulsion, drip monomer C and initiator D in stratum nucleare emulsion simultaneously, time for adding 1 ~ 3h, drip 75 ~ 85 DEG C, insulation reaction 2h, add polyaniline again and to dodecyl aminobenzoic acid, with salt acid for adjusting pH to 4, 75 ~ 85 DEG C of insulation reaction 1 ~ 3h, add metal-salt again, regulate pH to 4.0, 75 ~ 85 DEG C of insulation reaction time 1 ~ 2h, cool to 50 DEG C, add linking agent, reaction times 30min, add ammoniacal liquor adjust pH to 5, add dodecyl benzene sulfonyl chloride, temperature is regulated to be 75 ~ 85 DEG C, reaction 30min, obtain described fast light and germ resistance water soluble acrylic acid esters resin coating, gained acrylic resin coating has good photostabilization and germ resistance, and production technique environmental protection. |