titleOfInvention | Bollworm polyhedrosis protein extract is utilized to prepare the method for nanowires of gold |
abstract | A kind of method utilizing bollworm polyhedrosis protein extract to prepare nanowires of gold, it mainly uses ultra-pure water resuspended by after the centrifugal purification of former for heliothis armigera nuclear polyhedrosis virus powder, add alkali solution liquid process, add chloroform concussion more evenly, get abandoning supernatant after supernatant ultracentrifugation, add PBS solution and dissolve the precipitation spot stayed, then by gained solution adjust ph to 9 ~ 11,20 ~ 40 DEG C of hatching 20 ~ 30h, namely obtain polyhedrin extract; AuCl is added in the extract obtainedn 3 solution, fully mixes, in 20 ~ 40 DEG C, and shaking table hatching 20 ~ 25h under 130 ~ 170r/min; Dropwise add NaBHn 4 in 20 ~ 40 DEG C after solution reduces, under 130 ~ 170r/min, shaking table hatching 30 ~ 60h, obtains having cancellated nanowires of gold.Preparation technology of the present invention is simple, and cheaper starting materials is easy to get, and has very high biocompatibility, and obtained netted nanowires of gold pattern is even, Stability Analysis of Structures, can bear ultrasonic process and ultracentrifugation process. |
priorityDate | 2014-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |