titleOfInvention | A kind of fire-retardant preparation method with photostabilization nitrocellulose dope |
abstract | The invention discloses preparation method that is fire-retardant and photostabilization nitrocellulose dope, Mierocrystalline cellulose is immersed in water by it, adds chromium sulphate and photostabilization material, regulates temperature of reaction and pH, stirring reaction 2 ~ 4h, and gained liquid vacuum is dry, obtains pressed powder A; It is in the sulphuric acid soln of 60% that pressed powder A is immersed concentration, and at 50 ~ 85 DEG C of stirring reaction 3 ~ 5h, thin up makes reaction stop, and obtains reaction solution B; By centrifugal for reaction solution B, removing supernatant liquid, then adds water washing, more centrifugally obtains product C; In product C, add nitric acid, stirring reaction 3 ~ 5h under normal temperature, adds water and Saponin/TSM, is warmed up to 30 ~ 60 DEG C, then adds fire retardant, complexing agent and fermentation materials C, regulates pH to be 8, stirring reaction 1 ~ 2h, obtains fast light with flame retardant resistance coating; Gained coating is used as external and internal wall, furniture, the coating on hardware surface and paint. |