http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103951210-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C10-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C4-12 |
filingDate | 2014-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103951210-B |
titleOfInvention | Rare earth ion doped GdCl3Devitrified glass and preparation method thereof |
abstract | The invention discloses a kind of rare earth ion doped GdCl 3 Devitrified glass and preparation method thereof, its mole of percentage composition is P 2 O 5 :35-45mol%、GeO 2 :10-20mol%、NaF:15-23mol%、Gd 2 O 3 :5-9mol%、GdCl 3 :15-20mol%、LnCl 3 : 1-4mol%, wherein LnCl 3 For CeCl 3 、EuCl 3 、TbCl 3 、PrCl 3 、NdCl 3 In one, its preparation method is first to prepare P with fusion method 2 O 5 -GeO 2 -NaF-Gd 2 O 3 -GdCl 3 -LnCl 3 Be glass, after heat treatment obtain transparent GdCl 3 Devitrified glass, GdCl of the present invention 3 Devitrified glass, can Deliquescence-resistant, good mechanical property, short wavelength's royal purple light transmission rate be higher, has stronger light output, decay soon, the good performance such as energy resolution and temporal resolution. The preparation method of this devitrified glass is simple, and production cost is lower. |