http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103938193-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-18 |
filingDate | 2014-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103938193-B |
titleOfInvention | A kind of environmental protection high phosphorus chemical plating nickel liquid and application thereof for airtight glass sealing-in line terminals |
abstract | The invention discloses a kind of environmental protection high phosphorus chemical plating nickel liquid for airtight glass sealing-in line terminals, formed by the raw material of following concentration: nickelous sulfate: 25-27g/L, sodium hypophosphite: 19-22g/L, NaOH: 20-23g/L, lactic acid: 41-44g/L, trisodium citrate: 1.5-2.3g/L, malic acid: 13-15g/L, glycine: 8-12g/L, OP-10:0.2-0.4ml/L, stannous chloride: 0.26-0.3g/L, maleic anhydride: 0.26-0.34g/L, N, N-diethyl propargylamine: 3-5mg/L. The invention discloses a kind of method that adopts above-mentioned chemical nickel-plating liquid to carry out chemical plating. The present invention can make stainless pin and iron covering chemical nickel plating upper plating evenly simultaneously, ensures not produce any nickel core on sintered glass simultaneously, keeps the clean difficult problem of glass surface light thereby solved. |
priorityDate | 2014-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links