titleOfInvention | A kind of preparation method of the cellular film of nano-pore |
abstract | The preparation method that the invention discloses the cellular film of a kind of nano-pore.Selecting suitable solvent, configuration concentration is the polymer solution of 6mg/mL ~ 14mg/mL;Polymer solution being coated in substrate surface, is positioned in the room temperature atmospheric environment that relative humidity is 60% ~ 90%, stands 30 seconds ~ 4 minutes, namely prepare the cellular film with nano-pore structure after solvent volatilization completely, pore diameter range is 10 nanometers ~ 100 nanometers;Described solvent is Carbon bisulfide, chloroform, dichloromethane or toluene;Described substrate is silicon chip, glass, gold plaque, silver strip, mylar or Kapton.The inventive method, only by the linear polystyrene adopting double; two end group functional, can adopt spirogram method to prepare the cellular film with top layer nano-pore structure, and this is the minimum hole prepared by spirogram method up to now. |