classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-28 |
filingDate | 2014-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103865204-B |
titleOfInvention | A kind of preparation method of polychloroethylene pipes |
abstract | The invention discloses a kind of preparation method of polychloroethylene pipes, rotating speed raw materials all except titanium dioxide, CPE being poured into stirring tank 55-70 rev/min stirs mixed 1 hour, after put into twin screw extruder, mediate 8-10 minute at 140-150 DEG C after, add all the other raw materials by weight again, mixing, granulation, control temperature, at 150-160 DEG C, obtains finished product after moulding process; Gained pipe workpiece quality of the present invention is stablized, and smooth in appearance, intensity is good.Preparation technology of the present invention is energy-conservation, economy, environmental protection. |