http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103772985-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B7-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-92895 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2948-92704 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B7-7461 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-397 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-524 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 |
filingDate | 2012-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103772985-B |
titleOfInvention | A kind of high density modified matrix resin material and its production and use |
abstract | The invention belongs to technical field of polymer materials, relate to a kind of high density modified matrix resin material and its production and use.The material of the present invention is made up of the component comprising following weight portion: matrix resin 30 45 parts, high-density packing 55 70 parts, lubricant 0.4 0.7 parts, 0.2 0.4 parts of antioxidant, coupling agent 0.6 1 parts.Preparation method is as follows: by matrix resin 30 45 parts, high-density packing 55 70 parts, lubricant 0.4 0.7 parts, 0.2 0.4 parts of antioxidant, coupling agent 0.6 1 parts.Compared with prior art, the method have the advantages that (1) uses engineering plastics to add high-density packing, inertia disk can be met the requirement of density is ensured its mechanical property simultaneously;(2) engineering plastics have the advantages such as corrosion-resistant, acid and alkali-resistance, and its service life is better than traditional metal materials;(3) this kind of material integrated cost is less than traditional metal materials. |
priorityDate | 2012-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.