http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103771506-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W10-37 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G23-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J21-06 |
filingDate | 2013-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103771506-B |
titleOfInvention | Micro-/to receive hierarchy titanium dioxide microballoon sphere and preparation method thereof and application |
abstract | The invention discloses one and (included nano-particle by different nano units, nanometer sheet, nanometer rods) form micro-/receive hierarchy titanium dioxide microballoon sphere and preparation method thereof and application, it is mainly by carbamide, disodiumedetate, ammonium fluoride removes to control the hydrolysis of titanium source titanium sulfate, nucleation and crystallization process, by a step rapid microwave hydro-thermal reaction obtain micro-/receive the titanium dioxide microballoon sphere of hierarchy.This preparation method preparation process is simple, it is only necessary to is initially charged predecessor and further walks microwave hydrothermal and react, it is not necessary to subsequent treatment.This preparation technology response time is very short, and yield is big, it is easy to amplifies and produces.It can be widely used in and organic pollution is carried out light degradation process. |
priorityDate | 2013-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.