http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103769081-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fe23165b82e0c0988bab6c2beb449a00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-86 |
filingDate | 2012-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c890a0294d6ed48bfbcdf543d7b975e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_089a6514a38f7758c554c2fd71b2579f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1998e4f3837b06f319d9aa29aa96c6dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b93986e94256bf5c598f5e570aa0b526 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea1ab4dd8de1f9887fdd8525dcf27caf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9dae476ae90e44e4429abf458f5d7792 |
publicationDate | 2014-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-103769081-A |
titleOfInvention | Room temperature nitric oxide adsorption/ catalytic oxidation catalyst and preparation method thereof |
abstract | The invention provides a room temperature nitric oxide adsorption/ catalytic oxidation catalyst, and is characterized in that: the catalyst uses manganese cerium solid solution as an active component, the manganese cerium solid solution content is 100%, and the molar ratio of manganese to cerium is 2:3-1:1. The preparation method comprises the following steps: dissolving ammonium ceric nitrate and potassium permanganate in deionized water; dissolving manganese nitrate in the deionized water; dissolving a potassium hydroxide solution in the deionized water; pouring a manganese nitrate solution into an ammonium ceric nitrate and potassium permanganate mixed solution, using a mechanical stirrer for full and evenly stirring; heating the mixed solution to 70 to 80 DEG C for homoiothermy; dropwise adding a potassium hydroxide solution until the pH is 8-9; washing and drying a obtained sedimentation, and then baking at 300-400 DEG C for 3-4 hours to obtain the room temperature nitric oxide adsorption / catalytic oxidation catalyst. The method has the characteristics of simple preparation process, high adsorption / catalytic oxidation efficiency and the like. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105289641-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106540710-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113135552-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111774069-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111774069-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113351152-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112354535-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105633423-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104383916-A |
priorityDate | 2012-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.